Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 98.3 - 185 °C | 209 - 365 °F | Average value: 155 °C Grade Count:7 |
Overview of materials for Polystyrene + Polyphenylene Ether, Glass + Mineral Filler This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene + Polyphenylene Ether, Glass + Mineral Filler". Each property range of values reported is mi.. |