Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 291 °C | 555 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PA4/6 0206 Availability: North AmericaForms: PelletsFeatures: High Specific Gravity and Thermally ConductiveInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 291 °C @Thickness 3.20 mm |
556 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP VERTON UV00AS PPA (Asia Pacific) LNP* Verton* UV00AS is a compound based on Polyphthalamide resin containing Long Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 291 °C @Thickness 3.20 mm |
556 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP VERTON UV00ASU PPA LNP* VERTON* UV00ASU is a compound based on Polyphthalamide resin containing 50% Long Glass Fiber. Added features of this material include: UV Stabilized, Heat Stabilized, Structural. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 291 °C @Thickness 3.20 mm |
556 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP VERTON UV00AS PPA LNP* VERTON* UV00AS is a compound based on Polyphthalamide resin containing 50% Long Glass Fiber. Added features of this material include: Heat Stabilized, Structural. |