Techmer ES HiFill® PA4/6 0206

Category Polymer , Thermoplastic , Nylon , Nylon 46
Manufacturer Techmer ES
Trade Name HiFill®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Techmer ES HiFill® PA4/6 0206.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Availability: North AmericaForms: PelletsFeatures: High Specific Gravity and Thermally ConductiveInformation provided by TP Composites, Inc.
Physical Properties Metric English Comments
Density 2.06 g/cc
0.0744 lb/in³
ASTM D792
Water Absorption 0.10 %

@Time 86400 sec
0.10 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.015 cm/cm

@Thickness 3.17 mm
0.015 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Yield 106 MPa
15400 psi
ASTM D638
Elongation at Break 2.0 %
2.0 %
ASTM D638
Flexural Strength 180 MPa
26100 psi
ASTM D790
Flexural Modulus 10.3 GPa
1500 ksi
ASTM D790
Izod Impact, Notched 0.400 J/cm

@Thickness 3.17 mm
0.750 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 36.0 µm/m-°C
20.0 µin/in-°F
ASTM D696
Thermal Conductivity 0.980 W/m-K
6.80 BTU-in/hr-ft²-°F
ASTM C177
Deflection Temperature at 0.46 MPa (66 psi) 291 °C
555 °F
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 277 °C
530 °F
Unannealed; ASTM D648