Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 101 - 114 °C | 214 - 237 °F | with 160ºC thermal postcure; ASTM D648 |
3D Systems Accura® 40 Plastic for SLA® Systems 40 Accura "Nd" type material - for use with Viper SLA, and SLA 3500, 5000 and 7000 systems.ApplicationsHigh temperature testing:Automotive "under-the-hood" partsIntake manifoldsLighting components a.. |