Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 113 °C
236 °F
ASTM D648
Ineos H44N-00 Polypropylene Homopolymer
H44N-00 is a high flow rate, nucleated polypropylene homopolymer designed for compounding and injection molding applications. The grade benefits from a high stiffness and isotropic shrinkage to help..
Deflection Temperature at 0.46 MPa (66 psi) 113 °C
236 °F
ASTM D648
Plastics Group Polifil® RMT-10 10% Talc-Reinforced Polypropylene, High Impact
Polifil® RMT series compounds are high impact polypropylenes reinforced with asbestos-free talc. In addition to high impact strength, they possess a high flex modulus and high heat deflection resis..