Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 227 °C | 440 °F | ASTM D648 |
Polymer Resources PPX/NY G30 PPO/Nylon 66 Alloy , 30% Glass Reinforced Polyphenylene Oxide/Nylon 66 Alloy , 30% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informa.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 227 °C | 440 °F | Unannealed; ASTM D785 |
Ravago Manufacturing Americas Hylon® N1200THL BK Nylon 6/6 Available in North America Additive: Heat Stabilizer, Impact Modifier and Lubricant Features: Lubricated, Impact Modified and Heat StabilizedRoHS CompliantForm: Pellets Color: BlackInformation prov.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 227 °C | 440 °F | ASTM D648 |
Polymer Resources NY66-IM1 Nylon 66, Medium Impact Modified Nylon 66, Medium Impact Modified, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are te.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 227 °C | 440 °F | ASTM D648 |
Polymer Resources NY66-IM1-[color]-H Nylon 66, Medium Impact Modified, Heat Stabilized Nylon 66, Medium Impact Modified, Heat Stabilized, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Ny.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 227 °C | 440 °F | ASTM D648 |
Polymer Resources NY66-IM1-[color]H Nylon, Medium Impact Modified, Heat Stabilized (DAM) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 227 °C | 440 °F | ASTM D648 |
Polymer Resources NY6-M25G15-[color]-H Nylon 6, 25% Mineral, 15% Glass Reinforced, Heat Stabilized Nylon 6, 25% Mineral, 15% Glass Reinforced, Heat Stabilized, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test s.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 227 °C | 440 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PBT GF30 HR BK 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightFeatures: Hydrolysis ResistantAppearance: BlackInformation provided by TP Composites, In.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 227 °C | 441 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics LNP Thermocomp OF004AER PPS (Asia Pacific) LNP* Thermocomp* OF004AER is a compound based on Polyphenylene Sulfide resin containing Glass Fiber. Added features of this material include: Easy Molding, Mold Release.This data was supplied by SA.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 227 °C | 441 °F | ASTM D648 |
A. Schulman SCHULADUR® B GF25LB 25% Glass Fiber Reinforced, Lubricated PET Information provided by A. Schulman. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 227 °C | 441 °F | ASTM D648 |
A. Schulman ComAlloy® E-13370 Lubricated Reinforced Polyester Alloy Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 227 °C | 440 °F | ASTM D648 |
Plastics Group Polifil® 625L Nylon 6/6 (DAM) Polifil® NYLON 6/6 combines good abrasion and chemical resistance.Applications: ValvesBearingsBearing casesStandard processing techniques are applicable. Information provided by The Plastics Group... |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 227 °C | 441 °F | ASTM D648 |
A. Schulman SCHULADUR® B GF25LB 25% Glass Fiber Reinforced, Lubricated PET Information provided by A. Schulman. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 227 °C | 441 °F | ASTM D648 |
A. Schulman ComAlloy® E-13370 Lubricated Reinforced Polyester Alloy Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 227 °C | 441 °F | ASTM D648 |
A. Schulman SCHULADUR® B GF25LB 25% Glass Fiber Reinforced, Lubricated PET Information provided by A. Schulman. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 227 °C | 441 °F | ASTM D648 |
A. Schulman ComAlloy® E-13370 Lubricated Reinforced Polyester Alloy Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 227 °C | 441 °F | ASTM D648 |
A. Schulman ComAlloy® E-13370 Lubricated Reinforced Polyester Alloy Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 227 °C | 441 °F | ASTM D648 |
A. Schulman SCHULADUR® B GF25LB 25% Glass Fiber Reinforced, Lubricated PET Information provided by A. Schulman. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 227 °C | 441 °F | ASTM D648 |
A. Schulman ComAlloy® E-13370 Lubricated Reinforced Polyester Alloy Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 227 °C | 441 °F | ASTM D648 |
A. Schulman SCHULADUR® B GF25LB 25% Glass Fiber Reinforced, Lubricated PET Information provided by A. Schulman. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 227 °C | 441 °F | ASTM D648 |
A. Schulman SCHULADUR® B GF25LB 25% Glass Fiber Reinforced, Lubricated PET Information provided by A. Schulman. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 227 °C | 440 °F | ASTM D648 |
Clariant Renol 6601L Nylon 66, Lubricated Data provided by Clariant Masterbatches |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 227 °C | 441 °F | ASTM D648 |
Adell AJ-13 Nylon 66, 15% Glass Reinforced; High Impact Data provided by Adell Plastics, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 227 °C | 441 °F | ASTM D648 |
Ashley Polymers Ashlene® 526LD Nylon 66 Modified for toughness at low temperatures, injection molding grade.Data provided by the manufacturer |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 227 °C | 441 °F | ASTM D648 |
A. Schulman ComAlloy E-13370B Internally Lubricated, Glass Fiber Reinforced Polyester Alloy Data provided by the manufacturer, ComAlloy International Company. High performance and excellent lubricity with minimal surface wear.The ComAlloy product line has been integrated into the A Schulma.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 227 °C | 441 °F | ASTM D648 |
A. Schulman ComAlloy Hiloy® 415 Polyester - PBT, Glass Reinforced Data provided by the manufacturer, ComAlloy International Company.20% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 227 °C | 441 °F | ASTM D648 |
A. Schulman ComAlloy Comtuf® 631 Nylon 6/6, Glass Reinforced, Impact Modified Data provided by the manufacturer, ComAlloy International Company.13% Glass Reinforced. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has been int.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 227 °C | 440 °F | ASTM D648 |
Polymer Resources PPX/NY G30 Modified PPO, 30% Glass Reinforced PPX/Nylon 6,6 Alloy
(Unverified Data**)&l Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |