Ravago Manufacturing Americas Hylon® N1200THL BK Nylon 6/6

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, Heat Stabilized
Manufacturer Ravago Manufacturing Americas, LLC
Trade Name Hylon®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ravago Manufacturing Americas Hylon® N1200THL BK Nylon 6/6.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Available in North America Additive: Heat Stabilizer, Impact Modifier and Lubricant Features: Lubricated, Impact Modified and Heat StabilizedRoHS CompliantForm: Pellets Color: BlackInformation provided by Ravago.
Physical Properties Metric English Comments
Specific Gravity 1.11 g/cc
1.11 g/cc
ASTM D792
Water Absorption 1.2 %

@Time 86400 sec
1.2 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.017 - 0.021 cm/cm

@Thickness 3.17 mm
0.017 - 0.021 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 110
110
ASTM D785
Tensile Strength at Break 62.1 MPa
9000 psi
ASTM D638
Elongation at Break 25 %
25 %
ASTM D638
Flexural Strength 75.8 MPa
11000 psi
ASTM D790
Flexural Modulus 2.41 GPa
350 ksi
ASTM D790
Izod Impact, Notched 1.60 J/cm
3.00 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 227 °C
440 °F
Unannealed; ASTM D785
Deflection Temperature at 1.8 MPa (264 psi) 68.3 °C
155 °F
Unannealed; ASTM D648