Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 98.9 - 104 °C | 210 - 219 °F | Average value: 101 °C Grade Count:5 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), PTFE Filled". Each property range of values reported is minimum a.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 96.0 - 104 °C | 205 - 219 °F | |
C.O.I.M. EXTER S® S 110 Orthophthalic Resin Description: The Exter S product line contains a large number of unsaturated polyester resin products with an array of properties and applications.Specific Notes for ESTER S® S 110: Highly reactive.. |