Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 182 - 188 °C
360 - 370 °F
ASTM D648
Cast Nylons Nycast® GF 30% Glass Filled Cast Nylon
Offering improved tensile, compressive and flexural properties over conventional unfilled cast nylon, NYCAST® GF (Glass Filled)-30% provides increased load bearing characteristics and is the choice..
Deflection Temperature at 0.46 MPa (66 psi) 181 - 188 °C
358 - 370 °F
Average value: 185 °C Grade Count:6
Overview of materials for Polysulfone, 20% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polysulfone, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% are inc..