Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 71.7 °C | 161 °F | ASTM D648 |
ExxonMobil HDPE HD 6733.17 High Density Polyethylene Copolymer Resin Product Description: HD 6733 is a narrow molecular weight hexane copolymer designed to maximize injection molding speed and productivity in thing wall articles. Lower processing temperatures enable .. |