Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 98.0 µm/m-°C @Temperature >=132 °C |
54.4 µin/in-°F @Temperature >=270 °F |
above Tg |
Resinlab® EP1285HD-12 Highly Filled, Medium Viscosity Casting Resin Resinlab™ EP1285 (Formerly Lab Product W021901 series) is a highly filled, medium viscosity black casting resin designed for applications requiring a high degree of thermal conductivity and a low C.. |
|||
CTE, linear | 98.0 µm/m-°C @Temperature 5.00 - 20.0 °C |
54.4 µin/in-°F @Temperature 41.0 - 68.0 °F |
Below Tg |
3M Scotch-Weld™ DP125 Gray Epoxy Adhesive Scotch-Weld epoxy adhesive DP125 Gray is a filled, pigmented version of the Scotch-Weld epoxy adhesive DP125 Translucent and has similar performance and flexibility properties.Information provided b.. |