Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 90.5 µm/m-°C @Temperature 20.0 °C |
50.3 µin/in-°F @Temperature 68.0 °F |
Cured property; alpha 1; JMTP P200 |
Aptek 2506-A/B Room temperature curing, low modulus urethane conformal coating Room temperature curing, low modulus urethane conformal coatingAPTEK 2506-A/B is an unfilled, two component, electrically insulating, transparent, flexible urethane coating system designed for the e.. |