Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 9.58 µm/m-°C @Temperature 37.8 - 260 °C |
5.32 µin/in-°F @Temperature 100 - 500 °F |
|
Crucible Steel REX® M4 High Speed Steel REX M4 is a special purpose high speed steel designed to give high wear resistance in tools. Its high vanadium and carbon content provide for high resistance to cratering and wear in cold work punch.. |