Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 9.57 µm/m-°C @Temperature 24.0 - 316 °C |
5.32 µin/in-°F @Temperature 75.2 - 601 °F |
|
QuesTek® Innovations Ferrium® C64™ Case-hardened Gear Steel with Ultrahigh-strength Core Description: Ferrium® C64™ is a member of a new class of martensitic secondary-hardening gear and bearing steels that utilize an efficient M2C precipitate strengthening dispersion. Because of the .. |
|||
CTE, linear | 9.58 µm/m-°C @Temperature 37.8 - 260 °C |
5.32 µin/in-°F @Temperature 100 - 500 °F |
|
Crucible Steel REX® M4 High Speed Steel REX M4 is a special purpose high speed steel designed to give high wear resistance in tools. Its high vanadium and carbon content provide for high resistance to cratering and wear in cold work punch.. |