Polymer Property : CTE, linear = 9.400 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 16.92 µm/m-°C

@Temperature 25.0 - 1000 °C
9.400 µin/in-°F

@Temperature 77.0 - 1830 °F
Carpenter BioDur™ CCM Plus™ Medical Implant Alloy, Annealed 1093°C 1 hr
Data provided by Carpenter Technology Corporation.Annealing followed by water quench and low stress grinding prior to tensile testing.Medical Implant Alloy. Non-magnetic Co-Cr-Mo alloy exhibiting h..
CTE, linear 16.92 µm/m-°C

@Temperature 25.0 - 1000 °C
9.400 µin/in-°F

@Temperature 77.0 - 1830 °F
Carpenter BioDur™ CCM Plus™ Medical Implant Alloy, Annealed 1093°C 2 hr
Data provided by Carpenter Technology Corporation.Annealing followed by water quench and low stress grinding prior to tensile testing.Medical Implant Alloy. Non-magnetic Co-Cr-Mo alloy exhibiting h..
CTE, linear 16.92 µm/m-°C

@Temperature 25.0 - 1000 °C
9.400 µin/in-°F

@Temperature 77.0 - 1830 °F
Carpenter BioDur™ CCM Plus™ Medical Implant Alloy, Annealed 1121°C 1 hr
Data provided by Carpenter Technology Corporation.Annealing followed by water quench and low stress grinding prior to tensile testing.Medical Implant Alloy. Non-magnetic Co-Cr-Mo alloy exhibiting h..
CTE, linear 16.92 µm/m-°C

@Temperature 25.0 - 1000 °C
9.400 µin/in-°F

@Temperature 77.0 - 1830 °F
Carpenter BioDur™ CCM Plus™ Medical Implant Alloy, Annealed 1149°C (2100°F) 1 hr
Data provided by Carpenter Technology Corporation.Annealing followed by water quench and low stress grinding prior to tensile testing.Medical Implant Alloy. Non-magnetic Co-Cr-Mo alloy exhibiting h..
CTE, linear 16.92 µm/m-°C

@Temperature 25.0 - 1000 °C
9.400 µin/in-°F

@Temperature 77.0 - 1830 °F
Carpenter BioDur™ CCM Plus™ Medical Implant Alloy, Hot Worked
Data provided by Carpenter Technology Corporation.Medical Implant Alloy. Non-magnetic Co-Cr-Mo alloy exhibiting high strength, corrosion resistance, and wear resistance. BioDur CCM Plus alloy is a..