Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 151 µm/m-°C @Temperature 200 - 300 °C |
84.0 µin/in-°F @Temperature 392 - 572 °F |
ASTM E831 |
3M Dyneon™ CC605 PTFE 25% Fiberglass Filled
(discontinued **) Product Form: White, pelletized free-flowing powder. Applications include bearings, valve seats, seals.Data provided by Dyneon. |