3M Dyneon™ CC605 PTFE 25% Fiberglass Filled  (discontinued **)

Category Polymer , Thermoplastic , Fluoropolymer , PTFE , Polytetrafluoroethylene (PTFE), Glass Filled, Molded
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M Dyneon™ CC605 PTFE 25% Fiberglass Filled  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Form: White, pelletized free-flowing powder. Applications include bearings, valve seats, seals.Data provided by Dyneon.
Physical Properties Metric English Comments
Bulk Density 0.730 g/cc
0.0264 lb/in³
ASTM D4894
Density 2.22 g/cc
0.0802 lb/in³
ASTM D4894
Particle Size 750 µm
750 µm
ASTM D4894
Deformation 3.0 %

@Pressure 15.00 MPa
3.0 %

@Pressure 2175 psi
ASTM D621
7.0 %

@Time 86400 sec,
Pressure 15.00 MPa
7.0 %

@Time 24.0 hour,
Pressure 2175 psi
ASTM D621
Mechanical Properties Metric English Comments
Hardness, Shore D 57
57
value after 15 sec; ASTM D2240
62
62
initial value; ASTM D2240
Tensile Strength at Break 17.2 MPa
2490 psi
ASTM D4894
Elongation at Break 230 %
230 %
ASTM D4894
Tensile Modulus 0.159 GPa
23.0 ksi
ASTM D638
Thermal Properties Metric English Comments
CTE, linear 50.0 µm/m-°C

@Temperature 30.0 - 100 °C
27.8 µin/in-°F

@Temperature 86.0 - 212 °F
ASTM E831
122 µm/m-°C

@Temperature 100 - 200 °C
68.0 µin/in-°F

@Temperature 212 - 392 °F
ASTM E831
151 µm/m-°C

@Temperature 200 - 300 °C
84.0 µin/in-°F

@Temperature 392 - 572 °F
ASTM E831
Thermal Conductivity 0.290 W/m-K

@Temperature 100 °C
2.01 BTU-in/hr-ft²-°F

@Temperature 212 °F
ASTM E1530
0.300 W/m-K

@Temperature 250 °C
2.08 BTU-in/hr-ft²-°F

@Temperature 482 °F
ASTM E1530
Shrinkage 1.6 %
1.6 %
ASTM D4894