Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 149 µm/m-°C @Temperature 37.8 °C |
83.0 µin/in-°F @Temperature 100 °F |
ASTM E831 |
Arkema Group Solarkote® P-610 Acrylic PVC Capstock, clear, low glossInformation provided by Arkema Group |
|||
CTE, linear | 149 µm/m-°C @Temperature 37.8 °C |
83.0 µin/in-°F @Temperature 100 °F |
ASTM E831 |
Arkema Group Solarkote® P-600 Acrylic PVC Capstock, clear, high glossInformation provided by Arkema Group |
|||
CTE, linear | 149 µm/m-°C @Temperature 37.8 °C |
83.0 µin/in-°F @Temperature 100 °F |
ASTM E831 |
Arkema Group Solarkote® P-601 Acrylic PVC Capstock, white, high glossInformation provided by Arkema Group |
|||
CTE, linear | 149 µm/m-°C @Temperature 37.8 °C |
83.0 µin/in-°F @Temperature 100 °F |
ASTM E831 |
Arkema Group Solarkote® P-611 Acrylic PVC capstock, white, low glossInformation provided by Arkema Group |