Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 16.0 µm/m-°C @Temperature 0.000 - 100 °C |
8.90 µin/in-°F @Temperature 32.0 - 212 °F |
|
Crucible Steel 316L Chromium-Nickel Steel Crucible 316L is a non-hardenable, low carbon austenitic chromium-nickel steel with superior corrosion and heat resisting qualities. Crucible 316L is designed for special applications requiring resi.. |