Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 14.7 µm/m-°C @Temperature 25.0 - 700 °C |
8.18 µin/in-°F @Temperature 77.0 - 1290 °F |
|
Carpenter BioDur™ CCM Plus™ Medical Implant Alloy, Annealed 1093°C 1 hr Data provided by Carpenter Technology Corporation.Annealing followed by water quench and low stress grinding prior to tensile testing.Medical Implant Alloy. Non-magnetic Co-Cr-Mo alloy exhibiting h.. |
|||
CTE, linear | 14.7 µm/m-°C @Temperature 25.0 - 700 °C |
8.18 µin/in-°F @Temperature 77.0 - 1290 °F |
|
Carpenter BioDur™ CCM Plus™ Medical Implant Alloy, Annealed 1093°C 2 hr Data provided by Carpenter Technology Corporation.Annealing followed by water quench and low stress grinding prior to tensile testing.Medical Implant Alloy. Non-magnetic Co-Cr-Mo alloy exhibiting h.. |
|||
CTE, linear | 14.7 µm/m-°C @Temperature 25.0 - 700 °C |
8.18 µin/in-°F @Temperature 77.0 - 1290 °F |
|
Carpenter BioDur™ CCM Plus™ Medical Implant Alloy, Annealed 1121°C 1 hr Data provided by Carpenter Technology Corporation.Annealing followed by water quench and low stress grinding prior to tensile testing.Medical Implant Alloy. Non-magnetic Co-Cr-Mo alloy exhibiting h.. |
|||
CTE, linear | 14.7 µm/m-°C @Temperature 25.0 - 700 °C |
8.18 µin/in-°F @Temperature 77.0 - 1290 °F |
|
Carpenter BioDur™ CCM Plus™ Medical Implant Alloy, Annealed 1149°C (2100°F) 1 hr Data provided by Carpenter Technology Corporation.Annealing followed by water quench and low stress grinding prior to tensile testing.Medical Implant Alloy. Non-magnetic Co-Cr-Mo alloy exhibiting h.. |
|||
CTE, linear | 14.7 µm/m-°C @Temperature 25.0 - 700 °C |
8.18 µin/in-°F @Temperature 77.0 - 1290 °F |
|
Carpenter BioDur™ CCM Plus™ Medical Implant Alloy, Hot Worked Data provided by Carpenter Technology Corporation.Medical Implant Alloy. Non-magnetic Co-Cr-Mo alloy exhibiting high strength, corrosion resistance, and wear resistance. BioDur CCM Plus alloy is a.. |