Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 140 µm/m-°C @Temperature 200 - 300 °C |
78.0 µin/in-°F @Temperature 392 - 572 °F |
ASTM E831 |
3M Dyneon™ CCM605 PTFE, 25% Glass Filled
(discontinued **) Type II, free flowing.Typical Applications: Finished or semi-finished parts: sheets, rods, tubes, billets for skiving of films or machining into complex shapes.Information provided by the Dyneon div.. |
|||
CTE, linear | 140 µm/m-°C @Temperature 200 - 300 °C |
78.0 µin/in-°F @Temperature 392 - 572 °F |
ASTM E831 |
3M Dyneon™ CC655 PTFE, 50% Stainless Steel Filled
(discontinued **) Type II, free flowing.Typical Applications: Finished or semi-finished parts: sheets, rods, tubes, billets for skiving of films or machining into complex shapes.Information provided by the Dyneon div.. |
|||
CTE, linear | 140 µm/m-°C @Temperature 200 - 300 °C |
78.0 µin/in-°F @Temperature 392 - 572 °F |
ASTM E831 |
3M Dyneon™ CC646/S Custom Compound
(discontinued **) This compound consists of a mixture of 60% bronze blended with PTFE.Information provided by Dyneon, A 3M Company |
|||
CTE, linear | 140 µm/m-°C @Temperature 100 - 200 °C |
78.0 µin/in-°F @Temperature 212 - 392 °F |
ASTM E831 |
3M Dyneon™ CC085 Custom Fluoropolymer Compound
(discontinued **) This compound consists of a mixture of PPS and other proprietary fillers blended with PTFE.Information provided by Dyneon, A 3M Company |