Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 140 µm/m-°C @Temperature 23.0 - 100 °C |
77.8 µin/in-°F @Temperature 73.4 - 212 °F |
|
Murtfeldt Murinyl® Polyvinylidinefluoride As a fluorinated plastic, Murinyl® is exceptionally resistant to chemicals, hydrolysis, and sterilization. Its properties change very little at high service temperatures and after long-term exposur.. |
|||
CTE, linear | 140 µm/m-°C @Temperature >=143 °C |
77.8 µin/in-°F @Temperature >=289 °F |
Average above Tg; ISO 11359 |
Victrex® PEEK 150G / 151G Polyetheretherketone, Unreinforced Product Description:High performance thermoplastic material, unreinforced Polyetheretherketone (PEEK), semi crystalline, depth filtered granules for injection moulding, easy flow, FDA food contact c.. |
|||
CTE, linear | 140 µm/m-°C @Temperature >=143 °C |
77.8 µin/in-°F @Temperature >=289 °F |
Average above Tg; ISO 11359 |
Victrex® PEEK 150G903 Black Polyetheretherketone, Unreinforced Product Description:High performance thermoplastic material, unreinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding, easy flow, FDA food contact compliant, colou.. |
|||
CTE, linear | 140 µm/m-°C @Temperature >=143 °C |
77.8 µin/in-°F @Temperature >=289 °F |
Average above Tg; ISO 11359 |
Victrex® PEEK 450FE20 Polyetheretherketone, 20% PTFE Product Description:High performance thermoplastic material, 20% filled with PTFE Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding and extrusion, standard flow, FDA foo.. |
|||
CTE, linear | 140 µm/m-°C @Temperature >=143 °C |
77.8 µin/in-°F @Temperature >=289 °F |
Average above Tg; ISO 11357 |
Victrex® PEEK 450G General Purpose Product Description: High performance thermoplastic material, unreinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding and extrusion, standard flow, FDA food contac.. |
|||
CTE, linear | 140 µm/m-°C @Temperature >=143 °C |
77.8 µin/in-°F @Temperature >=289 °F |
Average above Tg; ISO 11359 |
Victrex® PEEK 90G Polyetheretherketone, Unreinforced Product Description:High performance thermoplastic material, unreinforced Polyetheretherketone (PEEK), semi crystalline, depth filtered granules for injection moulding, easy flow, FDA food contact c.. |
|||
CTE, linear | 140 µm/m-°C @Temperature 100 °C |
77.8 µin/in-°F @Temperature 212 °F |
|
Solvay Specialty Polymers Hyflon® PFA 450 Fluoropolymer
(discontinued **) Data provided by the manufacturer.Hyflon® PFA 450 has outstanding physical and chemical properties typical of fluoropolymers.Hyflon® PFA 420 |
|||
CTE, linear | 140 µm/m-°C @Temperature 200 - 300 °C |
78.0 µin/in-°F @Temperature 392 - 572 °F |
ASTM E831 |
3M Dyneon™ CCM605 PTFE, 25% Glass Filled
(discontinued **) Type II, free flowing.Typical Applications: Finished or semi-finished parts: sheets, rods, tubes, billets for skiving of films or machining into complex shapes.Information provided by the Dyneon div.. |
|||
CTE, linear | 140 µm/m-°C @Temperature 200 - 300 °C |
78.0 µin/in-°F @Temperature 392 - 572 °F |
ASTM E831 |
3M Dyneon™ CC655 PTFE, 50% Stainless Steel Filled
(discontinued **) Type II, free flowing.Typical Applications: Finished or semi-finished parts: sheets, rods, tubes, billets for skiving of films or machining into complex shapes.Information provided by the Dyneon div.. |
|||
CTE, linear | 140 µm/m-°C @Temperature 200 - 300 °C |
78.0 µin/in-°F @Temperature 392 - 572 °F |
ASTM E831 |
3M Dyneon™ CC646/S Custom Compound
(discontinued **) This compound consists of a mixture of 60% bronze blended with PTFE.Information provided by Dyneon, A 3M Company |
|||
CTE, linear | 140 µm/m-°C @Temperature 20.0 °C |
77.8 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Micropol Isoplas P501 Crosslinkable Polyethylene Information provided by Micropol Limited |
|||
CTE, linear | 140 µm/m-°C @Temperature 20.0 °C |
77.8 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Micropol Isoplas P651 Crosslinkable Polyethylene Information provided by Micropol Limited |
|||
CTE, linear | 140 µm/m-°C @Temperature 20.0 °C |
77.8 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Borealis BorPEX™ HE2515 High Density Polyethylene Compound for Silane Crosslinked Pipes BorPEX HE2515 is a silane crosslinkable compound which is used together with a catalyst masterbatch (Cat-MB) to accelerate the moisture-induced crosslinking reaction. It is designed for flexible cr.. |
|||
CTE, linear | 140 µm/m-°C @Temperature <=100 °C |
77.8 µin/in-°F @Temperature <=212 °F |
ISO E 830 |
Wolf Kunststoff ZEDEX® ZX-100EL63 A1G Polymer Alloy, Elastomer Modified Main Characteristics: Rubbery; Soft; High shock absorption; High impact resistance; Elongation > 300%Applications: Handling, Vessel and Pump, Steel and Water, Chemical Engineering, Automitve Technol.. |
|||
CTE, linear | 140 µm/m-°C @Temperature 110 - 150 °C |
77.8 µin/in-°F @Temperature 230 - 302 °F |
Above Tg |
Tra-Con Tra-Duct 921U02 Long Pot Life Silver-Filled Epoxy TRA-DUCT 921U02 long room temperature pot life, silver-filled epoxy. Information provided by Tra-Con Inc. |
|||
CTE, linear | 140 µm/m-°C @Temperature 20.0 °C |
77.8 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Borealis BorPEX™ ME2510 Medium Density Polyethylene Compound for Crosslinked Pipes (Pex-B (Silane)) BorPEX ME2510 is a silane crosslinkable compound which is used together with a catalyst masterbatch (Cat-MB) to accelerate the moisture-induced crosslinking reaction. It is designed for crosslinkab.. |
|||
CTE, linear | 140 µm/m-°C @Temperature 100 - 200 °C |
78.0 µin/in-°F @Temperature 212 - 392 °F |
ASTM E831 |
3M Dyneon™ CC085 Custom Fluoropolymer Compound
(discontinued **) This compound consists of a mixture of PPS and other proprietary fillers blended with PTFE.Information provided by Dyneon, A 3M Company |
|||
CTE, linear | 140 µm/m-°C @Temperature >=143 °C |
77.8 µin/in-°F @Temperature >=289 °F |
ISO 11359 |
Victrex® PEEK 381G Medium Viscosity Product Description: High performance thermoplastic material, unreinforced PolyEtherEtherKetone (PEEK), semi crystalline, depth filtered granules for specialty extrusion processes, standard flow, FD.. |
|||
CTE, linear | 140 µm/m-°C @Temperature >=143 °C |
77.8 µin/in-°F @Temperature >=289 °F |
Average above Tg; ISO 11359 |
Victrex® PEEK 450G903 Black Polyetheretherketone, Unreinforced Product Description:High performance thermoplastic material, unreinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding and extrusion, standard flow, FDA food contac.. |