Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 13.32 µm/m-°C @Temperature 21.0 - 649 °C |
7.400 µin/in-°F @Temperature 69.8 - 1200 °F |
|
Latrobe CBS-223â„¢ VIM-VAR Carburizing Bearing and Gear Steel CBS-223 VIM-VAR steel is a double vacuum melted carburizing steel with high hot hardness characteristics. Double vacuum melting sequentially combines vacuum induction melting with VACARCâ„¢ remel.. |