Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 13.0 µm/m-°C @Temperature 21.1 - 427 °C |
7.20 µin/in-°F @Temperature 70.0 - 800 °F |
H1150 |
Crucible Steel 15-5 Precipitation Hardening Stainless Steel Crucible 15-5 is a Premium Quality precipitation-hardening stainless steel which is capable of high strength and hardness levels after a relatively simple heat-treatment procedure. This grade is a V.. |
|||
CTE, linear | 13.0 µm/m-°C @Temperature 21.1 - 427 °C |
7.20 µin/in-°F @Temperature 70.0 - 800 °F |
H1150 |
Crucible Steel 17Cr-4Ni Precipitation Hardening Stainless Steel Crucible 17Cr-4Ni is a precipitation-hardening stainless steel which is capable of a high strength and hardness levels after a relatively simple heat-treatment procedure. This grade is martensitic a.. |
|||
CTE, linear | 13.0 µm/m-°C @Temperature 21.1 - 427 °C |
7.20 µin/in-°F @Temperature 70.0 - 800 °F |
H1150 |
Crucible Steel 17Cr-4Ni Super-X® Precipitation Hardening Stainless Steel Crucible 17Cr-4Ni is a version of 17CR-4Ni which has been modified to substantially improve machinability and other properties. Patented 17Cr-4Ni Super-X meets industry specifications for 17Cr-4Ni. .. |
|||
CTE, linear | 13.0 µm/m-°C @Temperature 20.0 - 316 °C |
7.20 µin/in-°F @Temperature 68.0 - 600 °F |
|
Crucible Steel CSM® 6 Tool Steel, AISI A6 CSM 6 is an air hardening tool steel offering moderate wear resistance and toughness. It may be hardened from a low hardening temperature for easy heat treatment.Information provided by Crucible Ind.. |
|||
CTE, linear | 13.0 µm/m-°C @Temperature 21.1 - 649 °C |
7.20 µin/in-°F @Temperature 70.0 - 1200 °F |
|
Crucible Steel HALCOMB® 425 Tool Steel, AISI H19 Halcomb 425 is designed for higher operating temperatures than H13, where wear resistance and heat check resistance are more critical than toughness. While H19 has excellent heat checking resistance.. |
|||
CTE, linear | 13.0 µm/m-°C @Temperature 21.1 - 204 °C |
7.20 µin/in-°F @Temperature 70.0 - 400 °F |
|
Schmolz + Bickenbach Cryodur® 2312 (Brake Die) Cold Work Die Steel Description: Cryodur® 2312 is a pre-hardened single melt Extra Fine Structure (EFS) plastic mold steel and Re-sulphurized to improve machinabilityCharacteristics: Excellent machinability compared t.. |
|||
CTE, linear | 13.0 µm/m-°C @Temperature 21.1 - 204 °C |
7.20 µin/in-°F @Temperature 70.0 - 400 °F |
|
Schmolz + Bickenbach Formadur® 2311 Plastic Mold Steel Description: Formadur® 2311 is a pre-hardened plastic mold steelCharacteristics: Good texturing compared to Formadur®2312 and Good polishability compared to Formadur® 231Applications: Injection m.. |
|||
CTE, linear | 13.0 µm/m-°C @Temperature 21.1 - 204 °C |
7.20 µin/in-°F @Temperature 70.0 - 400 °F |
|
Schmolz + Bickenbach Formadur® 2312 (Ultra Holder) Plastic Mold Steel Description: Formadur® 2312 is a pre-hardened single melt Extra Fine Structure (EFS) plastic mold steel and Re-sulphurized to improve machinabilityCharacteristics: Excellent machinability compared .. |