CTE, linear 118.2 - 126.2 µm/m-°C

@Temperature 95.0 - 110 °C
65.67 - 70.11 µin/in-°F

@Temperature 203 - 230 °F
RedEye On Demand Clear PolyJet™ FC720 for Rapid Prototyping
Clear PolyJet Resin (FC720) is a photopolymer resin designed for precise jetting in super fine layers by PolyJet™ Technology, often used in rapid prototyping. Our Clear PolyJet Resin material offer..