Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 64.8 µm/m-°C @Temperature 26.0 - 149 °C |
36.0 µin/in-°F @Temperature 78.8 - 300 °F |
Diameter |
Saint-Gobain Rulon® F Grade Bearing/Seal PTFE F Grade Bearing/Seal PTFE is used for applications requiring a long wearing material, especially in dry applications and those requiring high abrasion resistance. Standard tape liner material for Ru.. |