Material Notes:
F Grade Bearing/Seal PTFE is used for applications requiring a long wearing material, especially in dry applications and those requiring high abrasion resistance. Standard tape liner material for Rulon composite bearings. Green in color. Material has electrical and thermal insulation properties. Suitable for wet, dry or vacuum type environments. Mating surface of Rc 25 or higher steel. Markets for F grade include Appliances, Automotive, Document Processing Equipment, Industrial, Transportation.Rulon® is the Saint-Gobain trade name for their family of proprietary PTFE compounds. This family of materials offers the combination of high compressive strength, low coefficient of friction, and excellent abrasion and corrosion resistance while running without lubrication. A property of Rulon® is the absence of stick slip, that is, erratic low-speed motion.Information provided by Saint Gobain Performance Products.
Physical Properties Metric English Comments
Density 1.89 g/cc
0.0683 lb/in³
Deformation 3 %

@Temperature 23.0 °C,
Pressure 10.3 MPa
3 %

@Temperature 73.4 °F,
Pressure 1500 psi
24 hours
Mechanical Properties Metric English Comments
Tensile Strength 8.27 MPa
1200 psi
ASTM D638
Elongation at Break 160 %
160 %
ASTM D638
Compressive Yield Strength 6.89 MPa
1000 psi
Max load under tribological use
Coefficient of Friction, Dynamic 0.20
0.20
Coefficient of Friction, Static 0.12
0.12
Limiting Pressure Velocity 0.350 MPa-m/sec
10000 psi-ft/min
Thermal Properties Metric English Comments
CTE, linear 63.0 µm/m-°C

@Temperature 26.0 - 93.0 °C
35.0 µin/in-°F

@Temperature 78.8 - 199 °F
Diameter
64.8 µm/m-°C

@Temperature 26.0 - 149 °C
36.0 µin/in-°F

@Temperature 78.8 - 300 °F
Diameter
112 µm/m-°C

@Temperature 26.0 - 93.0 °C
62.0 µin/in-°F

@Temperature 78.8 - 199 °F
Length
126 µm/m-°C

@Temperature 26.0 - 149 °C
70.0 µin/in-°F

@Temperature 78.8 - 300 °F
Length
Thermal Conductivity 0.375 W/m-K
2.60 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 288 °C
550 °F
Minimum Service Temperature, Air -240 °C
-400 °F
Descriptive Properties Value Comments
Color Green