Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 6.80 µm/m-°C @Temperature 20.0 - 300 °C |
3.78 µin/in-°F @Temperature 68.0 - 572 °F |
|
Schott N-LAF36 Glass Information Provided by SCHOTT North America, Inc. |
|||
CTE, linear | 6.80 µm/m-°C @Temperature 20.0 - 300 °C |
3.78 µin/in-°F @Temperature 68.0 - 572 °F |
|
Schott N-SF66 Glass Information Provided by SCHOTT North America, Inc. |
|||
CTE, linear | 6.80 µm/m-°C @Temperature -30.0 - 70.0 °C |
3.78 µin/in-°F @Temperature -22.0 - 158 °F |
|
Schott N-SSK5 Glass Information Provided by SCHOTT North America, Inc. |
|||
CTE, linear | 6.80 µm/m-°C @Temperature 20.0 - 300 °C |
3.78 µin/in-°F @Temperature 68.0 - 572 °F |
|
Schott N-LAK10 Glass Information Provided by SCHOTT North America, Inc. |
|||
CTE, linear | 6.80 µm/m-°C @Temperature -30.0 - 70.0 °C |
3.78 µin/in-°F @Temperature -22.0 - 158 °F |
|
Schott N-LAK21 Glass Information Provided by SCHOTT North America, Inc. |
|||
CTE, linear | 6.80 µm/m-°C @Temperature 20.0 - 200 °C |
3.78 µin/in-°F @Temperature 68.0 - 392 °F |
|
CeramTec Rubalit® 708S Alumina, 96% Rubalit® 708S (96%) is an alumina that features high strength and thermal conductivity. It provides outstanding results when used on commercially available thick-film pastes and metallization syste.. |
|||
CTE, linear | 6.80 µm/m-°C @Temperature 20.0 - 200 °C |
3.78 µin/in-°F @Temperature 68.0 - 392 °F |
|
CeramTec Rubalit® 710 Alumina, 99.6% Rubalit® 710 (99.6%) is an alumina that produces optimum results and is considered the material of choice for thin-film technology. Its characterizing features are high strength and thermal conduct.. |
|||
CTE, linear | 6.80 µm/m-°C @Temperature 30.0 - 150 °C |
3.78 µin/in-°F @Temperature 86.0 - 302 °F |
|
Ametek Molybdenum-Copper Composite AMC 8515 Information supplied by Ametek Specialty Metal Products.The material is available as finished parts with the following maximum dimensions:Width: 6 inches (152 mm)Thickness: 0.150 inches (3.8 mm)Leng.. |
|||
CTE, linear | 6.80 µm/m-°C @Temperature 20.0 - 300 °C |
3.78 µin/in-°F @Temperature 68.0 - 572 °F |
ASTM-C372 |
CeramTec CeramCool® Rubalit® 708 Alumina, 96% CeramCool® is a metallized ceramic heat-sink for high power applications demonstrated by high power LED-systems. CeramCool® material characteristics: electrical insulation, high volume resistivit.. |
|||
CTE, linear | 6.80 µm/m-°C @Temperature 20.0 - 300 °C |
3.78 µin/in-°F @Temperature 68.0 - 572 °F |
DIN 51045 |
CeramTec Rubalit® 708 HP Alumina, 96% (High Performance) Rubalit® 708 HP (High Performance) has been developed from Rubalit® 708S. This material shares the same chemical composition, is produced on the same plant and using the identical production techn.. |