Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 12.2 µm/m-°C @Temperature 21.1 - 593 °C |
6.79 µin/in-°F @Temperature 70.0 - 1100 °F |
|
Crucible Steel CSM® S60V (440V) Tool Steel, AISI 440C Modified CPM S60V is a unique tool steel made by the Crucible Particle Metallurgy process. It is designed from a 440C stainless base analysis with added high carbon and vanadium for exceptionally good wear r.. |