Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 10.25 µm/m-°C @Temperature 24.0 - 538 °C |
5.694 µin/in-°F @Temperature 75.2 - 1000 °F |
|
QuesTek® Innovations Ferrium® C64™ Case-hardened Gear Steel with Ultrahigh-strength Core Description: Ferrium® C64™ is a member of a new class of martensitic secondary-hardening gear and bearing steels that utilize an efficient M2C precipitate strengthening dispersion. Because of the .. |