Thermal Properties Metric English Comments
CTE, linear 10.25 µm/m-°C

@Temperature 24.0 - 538 °C
5.694 µin/in-°F

@Temperature 75.2 - 1000 °F
QuesTek® Innovations Ferrium® C64™ Case-hardened Gear Steel with Ultrahigh-strength Core
Description: Ferrium® C64™ is a member of a new class of martensitic secondary-hardening gear and bearing steels that utilize an efficient M2C precipitate strengthening dispersion. Because of the ..