Polymer Property : CTE, linear = 5.567 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 10.02 µm/m-°C

@Temperature 250 °C
5.567 µin/in-°F

@Temperature 482 °F
Mykroy/Mycalex MM 601 Molding Grade Glass-bonded Mica Composite
Synthetic/Natural Mica Filler. Does not burn. ROHS Compliant.This ceramoplastic material is a versatile and efficient insulating material designed to meet the exacting demands of technical markets,..