Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 10.02 µm/m-°C @Temperature 250 °C |
5.567 µin/in-°F @Temperature 482 °F |
|
Mykroy/Mycalex MM 601 Molding Grade Glass-bonded Mica Composite Synthetic/Natural Mica Filler. Does not burn. ROHS Compliant.This ceramoplastic material is a versatile and efficient insulating material designed to meet the exacting demands of technical markets,.. |