Thermal Properties Metric English Comments
CTE, linear 8.00 - 9.50 µm/m-°C

@Temperature 25.0 - 100 °C
4.44 - 5.28 µin/in-°F

@Temperature 77.0 - 212 °F
Materion E40 Beryllium/BeO Composite, 40 Volume% BeO
Metal matrix composite made up principally of beryllium and crystal BeO platelets. Produced by blending the beryllium and beryllium oxide powders into a homogeneous mixture to create isotropic prop..