Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 5.20 µm/m-°C @Temperature 20.0 - 450 °C |
2.89 µin/in-°F @Temperature 68.0 - 842 °F |
|
H.C. Starck HPM 1800 Tungsten High Density Composite Description of Product: Tungsten based composite materials are outstanding due to high density and good mechanical properties. The product can be delivered both as semi-finished product for furthe.. |
|||
CTE, linear | 5.20 µm/m-°C @Temperature 20.0 - 100 °C |
2.89 µin/in-°F @Temperature 68.0 - 212 °F |
|
H.C. Starck HPM 1810 Tungsten High Density Composite Description of Product: Tungsten based composite materials are outstanding due to high density and good mechanical properties. The product can be delivered both as semi-finished product for furthe.. |
|||
CTE, linear | 5.20 µm/m-°C @Temperature 20.0 - 450 °C |
2.89 µin/in-°F @Temperature 68.0 - 842 °F |
|
H.C. Starck HPM 1850 Tungsten High Density Composite Description of Product: Tungsten based composite materials are outstanding due to high density and good mechanical properties. The product can be delivered both as semi-finished product for furthe.. |
|||
CTE, linear | 5.20 µm/m-°C @Temperature -30.0 - 70.0 °C |
2.89 µin/in-°F @Temperature -22.0 - 158 °F |
|
Schott KZFS12 Glass Information Provided by SCHOTT North America, Inc. |
|||
CTE, linear | 5.20 µm/m-°C @Temperature 20.0 - 300 °C |
2.89 µin/in-°F @Temperature 68.0 - 572 °F |
|
Schott N-ZK7 Glass Information Provided by SCHOTT North America, Inc. |
|||
CTE, linear | 5.20 µm/m-°C @Temperature 20.0 - 600 °C |
2.89 µin/in-°F @Temperature 68.0 - 1110 °F |
ASTM-C373 |
CeramTec Alunit® Aluminum Nitride Alunit® offers an extremely high thermal conductivity of 180 W/mK and outstanding electrical insulation properties. The thermal expansion coefficient of this material is comparable to silicon. Its .. |
|||
CTE, linear | 5.20 µm/m-°C @Temperature 20.0 - 600 °C |
2.89 µin/in-°F @Temperature 68.0 - 1110 °F |
ASTM-C372 |
CeramTec Alunit® HS Aluminum Nitride Alunit® HS offers an extremely high thermal conductivity of 170 W/mK and outstanding electrical insulation properties. The thermal expansion coefficient of this material is comparable to silicon. I.. |
|||
CTE, linear | 5.20 µm/m-°C @Temperature 25.0 - 400 °C |
2.89 µin/in-°F @Temperature 77.0 - 752 °F |
|
CoorsTek ACI-Ni6 Tungsten Carbide Applications: seal rings, plungers, liners, nozzles, valve components, pump components, wear components in the oil & gas, construction, and agriculture equipment industries |
|||
CTE, linear | 5.20 µm/m-°C @Temperature 20.0 - 600 °C |
2.89 µin/in-°F @Temperature 68.0 - 1110 °F |
ASTM-C372 |
CeramTec CeramCool® Alunit® Aluminum Nitride CeramCool® is a metallized ceramic heat-sink for high power applications demonstrated by high power LED-systems. CeramCool® material characteristics: electrical insulation, high volume resistivit.. |