Polymer Property : CTE, linear = 2.89 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 5.20 µm/m-°C

@Temperature 20.0 - 450 °C
2.89 µin/in-°F

@Temperature 68.0 - 842 °F
H.C. Starck HPM 1800 Tungsten High Density Composite
Description of Product: Tungsten based composite materials are outstanding due to high density and good mechanical properties. The product can be delivered both as semi-finished product for furthe..
CTE, linear 5.20 µm/m-°C

@Temperature 20.0 - 100 °C
2.89 µin/in-°F

@Temperature 68.0 - 212 °F
H.C. Starck HPM 1810 Tungsten High Density Composite
Description of Product: Tungsten based composite materials are outstanding due to high density and good mechanical properties. The product can be delivered both as semi-finished product for furthe..
CTE, linear 5.20 µm/m-°C

@Temperature 20.0 - 450 °C
2.89 µin/in-°F

@Temperature 68.0 - 842 °F
H.C. Starck HPM 1850 Tungsten High Density Composite
Description of Product: Tungsten based composite materials are outstanding due to high density and good mechanical properties. The product can be delivered both as semi-finished product for furthe..
CTE, linear 5.20 µm/m-°C

@Temperature -30.0 - 70.0 °C
2.89 µin/in-°F

@Temperature -22.0 - 158 °F
Schott KZFS12 Glass
Information Provided by SCHOTT North America, Inc.
CTE, linear 5.20 µm/m-°C

@Temperature 20.0 - 300 °C
2.89 µin/in-°F

@Temperature 68.0 - 572 °F
Schott N-ZK7 Glass
Information Provided by SCHOTT North America, Inc.
CTE, linear 5.20 µm/m-°C

@Temperature 20.0 - 600 °C
2.89 µin/in-°F

@Temperature 68.0 - 1110 °F
ASTM-C373
CeramTec Alunit® Aluminum Nitride
Alunit® offers an extremely high thermal conductivity of 180 W/mK and outstanding electrical insulation properties. The thermal expansion coefficient of this material is comparable to silicon. Its ..
CTE, linear 5.20 µm/m-°C

@Temperature 20.0 - 600 °C
2.89 µin/in-°F

@Temperature 68.0 - 1110 °F
ASTM-C372
CeramTec Alunit® HS Aluminum Nitride
Alunit® HS offers an extremely high thermal conductivity of 170 W/mK and outstanding electrical insulation properties. The thermal expansion coefficient of this material is comparable to silicon. I..
CTE, linear 5.20 µm/m-°C

@Temperature 25.0 - 400 °C
2.89 µin/in-°F

@Temperature 77.0 - 752 °F
CoorsTek ACI-Ni6 Tungsten Carbide
Applications: seal rings, plungers, liners, nozzles, valve components, pump components, wear components in the oil & gas, construction, and agriculture equipment industries
CTE, linear 5.20 µm/m-°C

@Temperature 20.0 - 600 °C
2.89 µin/in-°F

@Temperature 68.0 - 1110 °F
ASTM-C372
CeramTec CeramCool® Alunit® Aluminum Nitride
CeramCool® is a metallized ceramic heat-sink for high power applications demonstrated by high power LED-systems. CeramCool® material characteristics: electrical insulation, high volume resistivit..