Polymer Property : CTE, linear = 5.10 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 5.10 µm/m-°C

@Temperature 20.0 - 300 °C
2.83 µin/in-°F

@Temperature 68.0 - 572 °F
H.C. Starck HPM 1705 Tungsten High Density Composite
Description of Product: Tungsten based composite materials are outstanding due to high density and good mechanical properties. The product can be delivered both as semi-finished product for furthe..
CTE, linear 5.10 µm/m-°C

@Temperature 20.0 - 300 °C
2.83 µin/in-°F

@Temperature 68.0 - 572 °F
H.C. Starck HPM 1800 Tungsten High Density Composite
Description of Product: Tungsten based composite materials are outstanding due to high density and good mechanical properties. The product can be delivered both as semi-finished product for furthe..
CTE, linear 5.10 µm/m-°C

@Temperature 20.0 - 100 °C
2.83 µin/in-°F

@Temperature 68.0 - 212 °F
H.C. Starck HPM 1850 Tungsten High Density Composite
Description of Product: Tungsten based composite materials are outstanding due to high density and good mechanical properties. The product can be delivered both as semi-finished product for furthe..
CTE, linear 5.10 µm/m-°C

@Temperature 20.0 - 300 °C
2.83 µin/in-°F

@Temperature 68.0 - 572 °F
H.C. Starck HPM 1850 Tungsten High Density Composite
Description of Product: Tungsten based composite materials are outstanding due to high density and good mechanical properties. The product can be delivered both as semi-finished product for furthe..
CTE, linear 5.10 µm/m-°C

@Temperature 20.0 - 800 °C
2.83 µin/in-°F

@Temperature 68.0 - 1470 °F
Goodfellow Shapal™-M soft Aluminum Nitride (AlN) - Machinable
Shapal-M® soft is a high purity, machinable ceramic with high strength and high thermal conductivity. Although the thermal conductivity is not as high as Aluminum Nitride, it is still 50 times that..