Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 5.10 µm/m-°C @Temperature 20.0 - 300 °C |
2.83 µin/in-°F @Temperature 68.0 - 572 °F |
|
H.C. Starck HPM 1705 Tungsten High Density Composite Description of Product: Tungsten based composite materials are outstanding due to high density and good mechanical properties. The product can be delivered both as semi-finished product for furthe.. |
|||
CTE, linear | 5.10 µm/m-°C @Temperature 20.0 - 300 °C |
2.83 µin/in-°F @Temperature 68.0 - 572 °F |
|
H.C. Starck HPM 1800 Tungsten High Density Composite Description of Product: Tungsten based composite materials are outstanding due to high density and good mechanical properties. The product can be delivered both as semi-finished product for furthe.. |
|||
CTE, linear | 5.10 µm/m-°C @Temperature 20.0 - 100 °C |
2.83 µin/in-°F @Temperature 68.0 - 212 °F |
|
H.C. Starck HPM 1850 Tungsten High Density Composite Description of Product: Tungsten based composite materials are outstanding due to high density and good mechanical properties. The product can be delivered both as semi-finished product for furthe.. |
|||
CTE, linear | 5.10 µm/m-°C @Temperature 20.0 - 300 °C |
2.83 µin/in-°F @Temperature 68.0 - 572 °F |
|
H.C. Starck HPM 1850 Tungsten High Density Composite Description of Product: Tungsten based composite materials are outstanding due to high density and good mechanical properties. The product can be delivered both as semi-finished product for furthe.. |
|||
CTE, linear | 5.10 µm/m-°C @Temperature 20.0 - 800 °C |
2.83 µin/in-°F @Temperature 68.0 - 1470 °F |
|
Goodfellow Shapal™-M soft Aluminum Nitride (AlN) - Machinable Shapal-M® soft is a high purity, machinable ceramic with high strength and high thermal conductivity. Although the thermal conductivity is not as high as Aluminum Nitride, it is still 50 times that.. |