Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 88.2 µm/m-°C @Temperature 30.0 - 100 °C |
49.0 µin/in-°F @Temperature 86.0 - 212 °F |
ASTM E831 |
3M Dyneon™ CC191-HE Custom Fluoropolymer Compound
(discontinued **) This compound consists of a mixture of high elongation 23% carbon / 2% graphite blended with PTFE.Information provided by Dyneon, A 3M Company |
|||
CTE, linear | 88.2 µm/m-°C @Temperature 20.0 °C |
49.0 µin/in-°F @Temperature 68.0 °F |
ASTM D-696 |
Axiall 7055 Rigid PVC, Extrusion, White Georgia Gulf 7055 White is a special purpose rigid PVC extrusion compound designed for window and door applications. The compound exhibits the following characteristics: WeatherabilityChemical Res.. |