Thermal Properties Metric English Comments
CTE, linear 41.0 µm/m-°C

@Temperature 20.0 °C
22.8 µin/in-°F

@Temperature 68.0 °F
Temp range not reported; ASTM D696
Propex Fabrics Curv™ C100A Polypropylene/Polypropylene Thermoformable Composite
Curv™ key features include weight savings, total recyclability, no glass content, thermoformable, high impact strength, inertness, and abrasion resistance.Data provided by BP Amoco; Curv was spun o..
CTE, linear 41.0 µm/m-°C

@Temperature 50.0 - 200 °C
22.8 µin/in-°F

@Temperature 122 - 392 °F
DIN 53 752
Ensinger TECASINT 4201 SD Polyimide, Black, Carbon Fiber (PI)
TECASINT is a range of non-melting high temperature polyimides characterized by high strength over a wide range of temperatures, good long term thermal stability, minimal thermal expansion and excel..
CTE, linear 41.0 µm/m-°C

@Temperature 50.0 - 200 °C
22.8 µin/in-°F

@Temperature 122 - 392 °F
DIN 53 752
Ensinger TECASINT™ 2021 Polyimide, 15% Graphite (PI)
TECASINT™ 2000 series of polyimide stock shapes provide a superior combination of high temperature and bearing and wear, properties that make it an ideal choice for the most demanding applications...
CTE, linear 41.0 µm/m-°C

@Temperature 50.0 - 200 °C
22.8 µin/in-°F

@Temperature 122 - 392 °F
DIN 53 752
Ensinger TECASINT™ 2022 Polyimide, Black, 15% Graphite (PI)
TECASINT™ 2000 series of polyimide stock shapes provide a superior combination of high temperature and bearing and wear, properties that make it an ideal choice for the most demanding applications...