Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 41.0 µm/m-°C @Temperature 20.0 °C |
22.8 µin/in-°F @Temperature 68.0 °F |
Temp range not reported; ASTM D696 |
Propex Fabrics Curv™ C100A Polypropylene/Polypropylene Thermoformable Composite Curv™ key features include weight savings, total recyclability, no glass content, thermoformable, high impact strength, inertness, and abrasion resistance.Data provided by BP Amoco; Curv was spun o.. |
|||
CTE, linear | 41.0 µm/m-°C @Temperature 50.0 - 200 °C |
22.8 µin/in-°F @Temperature 122 - 392 °F |
DIN 53 752 |
Ensinger TECASINT 4201 SD Polyimide, Black, Carbon Fiber (PI) TECASINT is a range of non-melting high temperature polyimides characterized by high strength over a wide range of temperatures, good long term thermal stability, minimal thermal expansion and excel.. |
|||
CTE, linear | 41.0 µm/m-°C @Temperature 50.0 - 200 °C |
22.8 µin/in-°F @Temperature 122 - 392 °F |
DIN 53 752 |
Ensinger TECASINT™ 2021 Polyimide, 15% Graphite (PI) TECASINT™ 2000 series of polyimide stock shapes provide a superior combination of high temperature and bearing and wear, properties that make it an ideal choice for the most demanding applications... |
|||
CTE, linear | 41.0 µm/m-°C @Temperature 50.0 - 200 °C |
22.8 µin/in-°F @Temperature 122 - 392 °F |
DIN 53 752 |
Ensinger TECASINT™ 2022 Polyimide, Black, 15% Graphite (PI) TECASINT™ 2000 series of polyimide stock shapes provide a superior combination of high temperature and bearing and wear, properties that make it an ideal choice for the most demanding applications... |