Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 8.80 µm/m-°C @Temperature 20.0 - 450 °C |
4.89 µin/in-°F @Temperature 68.0 - 842 °F |
|
H.C. Starck MoCu 70/30 Molybdenum-Copper Composite Material Description of Product: Molybdenum-copper composite materials are produced by copper infiltration of porous sintered molybdenum. They are available with different copper contents (15 - 35 %). A t.. |
|||
CTE, linear | 8.80 µm/m-°C @Temperature 20.0 - 100 °C |
4.89 µin/in-°F @Temperature 68.0 - 212 °F |
|
H.C. Starck WCu 70/30 Tungsten-Copper Composite Material Description of Product: Tungsten-copper composite materials are produced by copper infiltration of porous sintered tungsten. They are available with different copper contents (10 - 30 %). A therm.. |
|||
CTE, linear | 8.80 µm/m-°C @Temperature 20.0 - 300 °C |
4.89 µin/in-°F @Temperature 68.0 - 572 °F |
|
Schott SF1 Glass Information Provided by SCHOTT North America, Inc. |
|||
CTE, linear | 8.80 µm/m-°C @Temperature 20.0 - 300 °C |
4.89 µin/in-°F @Temperature 68.0 - 572 °F |
|
Schott SF56A Glass Information Provided by SCHOTT North America, Inc. |
|||
CTE, linear | 8.80 µm/m-°C @Temperature 20.0 - 300 °C |
4.89 µin/in-°F @Temperature 68.0 - 572 °F |
|
Schott BG18 Band Pass Filter Ionically colored glass. Data provided by the manufacturer, Schott Glas Mainz. |
|||
CTE, linear | 8.80 µm/m-°C @Temperature 20.0 - 600 °C |
4.89 µin/in-°F @Temperature 68.0 - 1110 °F |
DIN 51045 |
CeramTec Rubalit® HSS Alumina, 75% (High Strength Substrate) Rubalit® HSS (High Strength Substrate) displays the successful union of elasticity and strength. The ultrafine microstructure of Rubalit® HSS is the basis for its outstanding substrate surface qua.. |
|||
CTE, linear | 8.80 µm/m-°C @Temperature 20.0 - 1000 °C |
4.89 µin/in-°F @Temperature 68.0 - 1830 °F |
DIN EN 821-1 |
CeramTec V 38 Alumina, 96.0% Al2O3-SiO2 Aluminas exhibit good mechanical properties such as hardness, compressive and tensile strength, and elastic modulus. They perform well at elevated temperatures. |
|||
CTE, linear | 8.80 µm/m-°C @Temperature 20.0 - 100 °C |
4.89 µin/in-°F @Temperature 68.0 - 212 °F |
|
TIMET TIMETAL® 550 (Ti-4Al-4Mo-2Sn) Titanium Alloy Solution Treated High-Strength Forging AlloyIndustry Specifications: Germany Aerospace: 3.7184. France: T-A4DE. UK Aerospace Specifications BS TA. 45, 46, 47, 48,49, 50, 51, 57.Features: TIMETAL 550, like TIMETAL.. |
|||
CTE, linear | 8.80 µm/m-°C @Temperature 20.0 - 100 °C |
4.89 µin/in-°F @Temperature 68.0 - 212 °F |
|
TIMET TIMETAL® 550 (Ti-4Al-4Mo-2Sn) Titanium Alloy Solution Treated and Aged High-Strength Forging AlloyIndustry Specifications: Germany Aerospace: 3.7184. France: T-A4DE. UK Aerospace Specifications BS TA. 45, 46, 47, 48,49, 50, 51, 57.Features: TIMETAL 550, like TIMETAL.. |
|||
CTE, linear | 8.80 µm/m-°C @Temperature -30.0 - 70.0 °C |
4.89 µin/in-°F @Temperature -22.0 - 158 °F |
|
Schott BG3 Band Pass Filter Ionically colored glass. Data provided by the manufacturer, Schott Glas Mainz. |
|||
CTE, linear | 8.80 µm/m-°C @Temperature 20.0 - 300 °C |
4.89 µin/in-°F @Temperature 68.0 - 572 °F |
|
Schott GG400 Long Pass Filter Colloidally colored glass. Data provided by the manufacturer, Schott Glas Mainz.Similar glasses include GG395, GG385, GG420, GG435, GG455, GG475, GG495, OG515, OG530, OG550, OG570, OG590, RG610, RG6.. |
|||
CTE, linear | 8.80 µm/m-°C @Temperature -30.0 - 70.0 °C |
4.89 µin/in-°F @Temperature -22.0 - 158 °F |
|
Schott BG26 Band Pass Filter Ionically colored glass. Data provided by the manufacturer, Schott Glas Mainz. |