Schott BG3 Band Pass Filter

Category Ceramic , Glass , Optical , Filter
Manufacturer Schott Glas Mainz
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Schott BG3 Band Pass Filter.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Ionically colored glass. Data provided by the manufacturer, Schott Glas Mainz.
Physical Properties Metric English Comments
Density 2.56 g/cc
0.0925 lb/in³
Thermal Properties Metric English Comments
CTE, linear 8.80 µm/m-°C

@Temperature -30.0 - 70.0 °C
4.89 µin/in-°F

@Temperature -22.0 - 158 °F
10.2 µm/m-°C

@Temperature 20.0 - 300 °C
5.67 µin/in-°F

@Temperature 68.0 - 572 °F
Transformation Temperature, Tg 478 °C
892 °F
Optical Properties Metric English Comments
Refractive Index 1.50

@Wavelength 1014 nm
1.50

@Wavelength 1014 nm
Hg
1.51

@Wavelength 587.6 nm
1.51

@Wavelength 587.6 nm
He
1.52

@Wavelength 435.8 nm
1.52

@Wavelength 435.8 nm
Hg
1.55

@Wavelength 302.1 nm
1.55

@Wavelength 302.1 nm
Hg
Transmission, Visible <= 1.0 %

@Wavelength 510 - 6801 nm
<= 1.0 %

@Wavelength 510 - 6801 nm
87 %

@Wavelength 400 nm
87 %

@Wavelength 400 nm
Internal transmittance of 95% at 400 nm
IR Transmittance 91 %

@Wavelength 750 - 900 nm
91 %

@Wavelength 750 - 900 nm
Internal transmittance of 99% from 750-900 nm.
UV Transmittance <= 0.0060 %

@Wavelength 200 - 250 nm
<= 0.0060 %

@Wavelength 200 - 250 nm
91 %

@Wavelength 340 - 370 nm
91 %

@Wavelength 340 - 370 nm
Internal transmittance of 99% from 340-370 nm
Reflection Coefficient, Visible (0-1) 0.92
0.92
Chemical Properties Metric English Comments
Acid Class, SR 1
1
Alkali Class, AR 1
1
Stain Resistance Class, FR 0.0
0.0