Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 8.40 µm/m-°C @Temperature 20.0 - 1000 °C |
4.67 µin/in-°F @Temperature 68.0 - 1830 °F |
60° to c-axis |
MarkeTech Sapphire (Aluminum Oxide - Al2O3) Single Crystal Data provided by the supplier, MarkeTech International.Sapphire is grown by several methods: Boule form (Czochralski), in plate form, or as tubes, rods and plates. Boules are grown up to 8" diam.. |
|||
CTE, linear | 8.40 µm/m-°C @Temperature -30.0 - 70.0 °C |
4.67 µin/in-°F @Temperature -22.0 - 158 °F |
|
Schott K7 Glass Information Provided by SCHOTT North America, Inc. |
|||
CTE, linear | 8.40 µm/m-°C @Temperature -30.0 - 70.0 °C |
4.67 µin/in-°F @Temperature -22.0 - 158 °F |
|
Schott N-BAF51 Glass Information Provided by SCHOTT North America, Inc. |
|||
CTE, linear | 8.40 µm/m-°C @Temperature 20.0 - 300 °C |
4.67 µin/in-°F @Temperature 68.0 - 572 °F |
|
Schott N-BALF5 Glass Information Provided by SCHOTT North America, Inc. |
|||
CTE, linear | 8.40 µm/m-°C @Temperature 20.0 - 300 °C |
4.67 µin/in-°F @Temperature 68.0 - 572 °F |
|
Schott N-LASF9 Glass Information Provided by SCHOTT North America, Inc. |
|||
CTE, linear | 8.40 µm/m-°C @Temperature 20.0 - 300 °C |
4.67 µin/in-°F @Temperature 68.0 - 572 °F |
|
Schott SF10 Glass Information Provided by SCHOTT North America, Inc. |
|||
CTE, linear | 8.40 µm/m-°C @Temperature -30.0 - 70.0 °C |
4.67 µin/in-°F @Temperature -22.0 - 158 °F |
|
Schott SF2 Glass Information Provided by SCHOTT North America, Inc. |
|||
CTE, linear | 8.40 µm/m-°C @Temperature 20.0 - 300 °C |
4.67 µin/in-°F @Temperature 68.0 - 572 °F |
|
Schott N-LAF7 Glass Information Provided by SCHOTT North America, Inc. |
|||
CTE, linear | 8.40 µm/m-°C @Temperature 25.0 - 1000 °C |
4.67 µin/in-°F @Temperature 77.0 - 1830 °F |
ASTM-C372 |
CoorsTek ADOS-90R 91% Alumina Thick Film Substrate This 91-percent alumina (nominal) formulation offers a dark brown body for special applications. Applications: thick films and lasers |
|||
CTE, linear | 8.40 µm/m-°C @Temperature 30.0 - 800 °C |
4.67 µin/in-°F @Temperature 86.0 - 1470 °F |
|
Ametek Molybdenum-Copper Composite AMC 7525 Information supplied by Ametek Specialty Metal Products.The material is available as finished parts with the following maximum dimensions:Width: 6 inches (152 mm)Thickness: 0.150 inches (3.8 mm)Leng.. |