Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 4.60 - 5.20 µm/m-°C @Temperature 20.0 - 400 °C |
2.56 - 2.89 µin/in-°F @Temperature 68.0 - 752 °F |
|
Special Metals NILO® Alloy K Controlled-Expansion Alloy Inflection point 450°C. A nickel-iron-cobalt controlled-expansion alloy containing 29% nickel. Its coefficient of expansion, which decreases with rising temperature to the inflection point, mat.. |
|||
CTE, linear | 4.60 µm/m-°C @Temperature 20.0 - 1000 °C |
2.56 µin/in-°F @Temperature 68.0 - 1830 °F |
DIN EN 821-1 |
CeramTec Rocar® S Silicon Carbide, SSiC Rocar® is an extremely lightweight silicon carbide ceramic. It permits a reduction in mass forces at high speeds, and is considered for its hardness, excellent resistance to corrosion and sudden ch.. |
|||
CTE, linear | 4.60 µm/m-°C @Temperature 20.0 - 1000 °C |
2.56 µin/in-°F @Temperature 68.0 - 1830 °F |
DIN EN 821-1 |
CeramTec Rocar® ST Silicon Carbide, SSiC Silicon carbide is extremely hard and displays excellent corrosion and thermal shock resistance. Its outstanding sliding properties and high thermal conductivity make useful in tribological applicat.. |
|||
CTE, linear | 4.60 µm/m-°C @Temperature 20.0 - 400 °C |
2.56 µin/in-°F @Temperature 68.0 - 752 °F |
|
CMW® 3950 AMS-T-21014 ASTM B777 High Density Machinable Tungsten Uses: Radiation Shielding, High Mass, Gyro, Ordnance. Machinability is similar to gray iron.Information provided by CMW Inc. |