Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 51.3 - 70.3 µm/m-°C @Temperature 40.0 - 70.0 °C |
28.5 - 39.1 µin/in-°F @Temperature 104 - 158 °F |
|
RedEye On Demand Clear PolyJet™ FC720 for Rapid Prototyping Clear PolyJet Resin (FC720) is a photopolymer resin designed for precise jetting in super fine layers by PolyJet™ Technology, often used in rapid prototyping. Our Clear PolyJet Resin material offer.. |