Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 63.0 µm/m-°C @Temperature 26.0 - 93.0 °C |
35.0 µin/in-°F @Temperature 78.8 - 199 °F |
Diameter |
Saint-Gobain Rulon® F Grade Bearing/Seal PTFE F Grade Bearing/Seal PTFE is used for applications requiring a long wearing material, especially in dry applications and those requiring high abrasion resistance. Standard tape liner material for Ru.. |
|||
CTE, linear | 63.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
35.0 µin/in-°F @Temperature -22.0 - 86.0 °F |
DIN 53752 |
Styron INSPIREâ„¢ TF0808S(U) Polypropylene TF0808S(U) is a talc filled PP exhibiting high impact resistance and a high stiffness. It is particularly well suited for low wall thickness bumper skins. INSPIRE TF0808S for painted parts INSPIRE .. |
|||
CTE, linear | 63.0 µm/m-°C @Temperature -40.0 - 0.000 °C |
35.0 µin/in-°F @Temperature -40.0 - 32.0 °F |
UV Postcure; ASTM E831-05 |
DSM Somos® GP Plus 14122 Somos® GP Plus 14122 is a low-viscosity stereolithography resin with an opaque white appearance. This material mirrors production plastics like ABS and PBT, making it an ideal choice for virtually .. |