Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 237 µm/m-°C @Temperature 0.000 - 100 °C |
132 µin/in-°F @Temperature 32.0 - 212 °F |
Z-Direction; IPC-TM-650 2.4.41 |
Rogers Corporation RT/duroid® 5880 Glass Microfiber Reinforced PTFE High Frequency Laminate RT/duroid® 5870 and 5880 glass microfiber reinforced PTFE composites are designed for exacting stripline and microstrip circuit applications. Glass reinforcing microfibers are randomly oriented to.. |