Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 190 - 220 µm/m-°C @Temperature >=180 °C |
106 - 122 µin/in-°F @Temperature >=356 °F |
Z-Direction; IPC-TM-650 2.4.24 |
Rogers Corporation Theta® MCL-HE-679G Laminate, GHA-679G Prepreg Halogen-Free, Low Dielectric Constant, High heat Resistant Multi-Layer Circuit Material Theta® circuit materials are halogen free and have good dielectric characteristics suitable for high speed digital applications. Theta materials, in part due to their superior heat resistance, hav.. |