Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 18.5 - 19.5 µm/m-°C @Temperature 20.0 - 200 °C |
10.3 - 10.8 µin/in-°F @Temperature 68.0 - 392 °F |
|
PEAK Werkstoff DISPAL S232 Aluminum Alloy, AlSi17Fe4Cu3Mg, Condition T6 Heat Treatment Condition T6 (Quench in water at RT). Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials allo.. |
|||
CTE, linear | 18.5 - 19.5 µm/m-°C @Temperature 20.0 - 200 °C |
10.3 - 10.8 µin/in-°F @Temperature 68.0 - 392 °F |
|
PEAK Werkstoff DISPAL S232 Aluminum Alloy, AlSi17Fe4Cu3Mg, Condition T6x Heat Treatment Condition T6x (Quench in water at RT). Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials all.. |